Caracteristici magnetice SmCo 

T
i
p

 
Material BH (max) Br (min-max) Forță coercitivă  Hcb
(min-max)
Fortă coercitivă internă
Hcj
(min-max)
Densitate

Temperatură

 tolerată

KJ/m3 MGoe T KGs KA/m KOe KA/m KOe g/cm3
SmCo5 XG16 120-143 15-18 0.77-0.86 7.7-8.6 613-716 7.7-9.0 ≧1194 ≧15 8.3 250
XG16H 120-143 15-18 0.77-0.86 7.7-8.6 613-716 7.7-9.0 ≧1592 ≧20
XG18 135-159 17-20 0.81-0.92 8.1-9.2 637-756 8.0-9.5 ≧1194 ≧15
XG18H 135-159 17-20 0.81-0.92 8.1-9.2 637-756 8.0-9.5 ≧1592 ≧20
XG20 151-175 19-22 0.85-0.95 8.5-9.5 637-756 8.0-9.5 ≧1194 ≧15
XG20H 151-175 19-22 0.85-0.95 8.5-9.5 637-756 8.0-9.5 ≧1592 ≧20
XG22 167-191 21-24 0.89-1.00 8.9-10 661-772 8.3-9.7 ≧1194 ≧15
XG22H 167-191 21-24 0.89-1.00 8.9-10 661-772 8.3-9.7 ≧1592 ≧20
Sm2Co17 XGS24M 175-199 22-25 0.92-1.04 9.2-10.4 318-788 4.0-9.9 398-1194 5.0-15.0 8.4 350
XGS24 175-199 22-25 0.92-1.04 9.2-10.4 661-796 8.3-10.0 1194-1990 15.0-25.0
XGS24H 175-199 22-25 0.92-1.04 9.2-10.4 661-804 8.3-10.1 ﹥1990 ﹥25.0
XGS26M 191-215 24-27 1.00-1.06 10.0-10.6 318-796 4.0-10.0 398-1194 5.0-15.0
XGS26 191-215 24-27 1.00-1.06 10.0-10.6 677-820 8.5-10.3 1194-1990 15.0-25.0
XGS26H 191-215 24-27 1.00-1.06 10.0-10.6 677-820 8.5-10.3 ﹥1990 ﹥25.0
XGS28M 207-231 26-29 10.4-11.0 10.4-11.0 318-804 4.0-10.1 398-1194 5.0-15.0
XGS28 207-231 26-29 10.4-11.0 10.4-11.0 677-820 8.5-10.3 1194-1990 15.0-25.0
XGS28H 207-231 26-29 10.4-11.0 10.4-11.0 677-820 8.5-10.3 ﹥1990 ﹥25.0
XGS30M 223-247 28-31 10.7-11.2 10.7-11.2 318-804 4.0-10.1 398-1194 5.0-15.0
XGS30 223-247 28-31 10.7-11.2 10.7-11.2 700-828 8.8-10.4 1194-1990 15.0-25.0
XGS30H 223-247 28-31 10.7-11.2 10.7-11.2 700-828 8.8-10.4 ﹥1990 ﹥25.0
XGS32M 231-255 29-32 10.9-11.5 10.9-11.5 318-804 4.0-10.1 398-955 5.0-12.0
XGS32 231-255 29-32 10.9-11.5 10.9-11.5 716-836 9.0-10.5 ﹥955 ﹥12.0
XGS22LT 159-183 20-23 9.0-9.9 9.0-9.9 677-756 8.5-9.5 ≧1194 ≧15.0
XGS24LT 159-183 20-23 9.2-10.2 9.2-10.2 677-756 8.5-9.5 ≧1194 ≧15.0